Gas atomization creates 15-45μm Type 4 powder. Sphericity >95% zaisťuje tlač . obsah kyslíka<100ppm prevents oxidation. Particle size distribution: 90% within ±5μm. Alloy composition controlled to ±0.2%. Advanced methods: Ultrasonic atomization for finer powders. Quality checks: SEM analysis and Hall flowmeter testing.